+86-18862679789
admin@evertopest.com
Content
A curtainwall carries no floor load. It hangs off the slab edge, seals the envelope, and hands wind, rain and thermal movement back to the frame. That single fact explains most of the arguments that appear later in a facade package, and most of the cost as well.
The short answer before the detail: on most mid-rise and high-rise projects, the infill panel decides the curtainwall, not the mullion. A 4 mm metal composite panel with an A2 non-combustible mineral core and a B1 flame-retardant panel look identical on a sample board, weigh almost the same, and sit within a few percentage points of each other on price. They behave completely differently in a fire test, in a specification review, and in an insurance file. Choosing between them is rarely a materials question. It is a documentation and manufacturing-control question, and that is where most facade packages quietly succeed or quietly go wrong.
This guide is written for the people who actually have to make that choice: facade consultants, panel manufacturers, importers, and the engineers who sign off the shop drawings. It covers what a curtainwall does, where composite panels fit, how the core class changes everything, what the production line has to hold to make the promise true, and the checks worth running before a purchase order is issued.
A curtainwall is a non-structural exterior envelope. It is fixed to the building structure, usually at the slab edge or to a supporting frame, but it does not contribute to the stability of the building. It is designed to move. Vertical movement from slab deflection, horizontal movement from wind and seismic drift, and thermal expansion of the aluminium all have to be absorbed inside the system, not transferred into it.
That is the opposite of a load-bearing wall, and it changes how every component is judged. A heavy stone facade is stable because it is thick. A curtainwall is stable because it is tolerant, and tolerance is expensive.
In practice a curtainwall has to do six jobs at once:
Notice what is missing from that list: appearance. Appearance matters enormously, but it is the outcome of the six jobs above, not a separate requirement. A facade that looks perfectly straight on handover and leaks in the third rainy season was never a good curtainwall; it just had not been tested yet.
This is also where the distinction from a window wall becomes practical rather than academic. A window wall sits between the slab edges, one bay at a time, and the slab is visible from the outside. A curtainwall runs continuously in front of the slab. The structural consequence is that a true curtainwall needs a slab edge cover, a fire stop at each floor line, and a bracket system that can absorb movement in three directions. The panel consequence is that the infill is exposed across a much larger continuous area, so flatness, colour consistency and joint alignment become visible at a distance where a window wall's imperfections would be hidden.
Curtainwall infill is a family, not a single product. Glass dominates commercial towers because it delivers daylight and a clean architectural line. Beyond glass, the common options are metal composite panels, aluminium honeycomb panels, corrugated aluminium panels, fibre cement, terracotta, and stone veneer on a carrier.
Metal composite panels earn their place for three reasons. First, flatness: a composite sandwich with a continuous mineral or polymer core holds a flatter surface over a 1.5 m span than a single aluminium sheet of the same thickness, which is why large format panels remain visually acceptable. Second, weight: a 4 mm composite panel is roughly a fifth of the mass of an equivalent glass unit or a stone panel, which reduces mullion size, bracket count and slab edge reinforcement. Third, fabrication: the panel can be routed, folded and returned to form a boxed edge, giving a crisp shadow line without a separate capping profile.
The chart below compares indicative panel mass per square metre across the most common infill types. The values are order-of-magnitude figures used for preliminary sizing, not catalogue data; every project should confirm the actual figure from the supplier's technical sheet.
The spread matters more than any single number. Moving from stone to a composite panel removes well over 30 kg per square metre of dead load across the facade, which feeds directly into mullion profiles, anchor design and the amount of edge reinforcement the slab needs. On a tall building the accumulated effect is significant, and it is often the reason composite panels appear on the upper floors even where stone is used at street level.
Weight is also the reason A2 and B1 panels are so often treated as interchangeable in a commercial discussion. The mass difference between a mineral-filled A2 core and a flame-retardant B1 core is small, typically well under 2 kg per square metre at 4 mm. The difference in fire behaviour is not small at all, and it is not visible from the outside of the building at any point in its life.
Composite panels carry one more practical advantage that rarely makes it into the specification: repairability. A damaged panel in a unitized system can usually be removed and replaced from the outside without disturbing adjacent units, provided the panel has been designed with a removable pressure plate or a compatible glazed-in detail. Stone and glass do not offer that convenience at the same cost.
From the outside, every metal composite panel is a thin aluminium skin, a core, and another thin aluminium skin, bonded under heat and pressure. The skin is almost always 0.3 mm to 0.5 mm alloy, usually 3003 or 5005, coated with polyester, PVDF or FEVE. The variable that decides fire performance, price and specification acceptance is the core.
An A2 non-combustible core is a mineral-filled compound, typically above 90 percent inorganic content by mass, based on magnesium hydroxide or aluminium hydroxide with a small polymer binder. It does not sustain combustion, contributes very little heat release, and is classified in the highest practical band for a composite panel under European and Chinese systems. A B1 flame-retardant core raises the inorganic filler to roughly 70 percent, which reduces but does not eliminate the contribution to fire. An ordinary polyethylene core, sometimes called B2 or standard, is essentially a plastic sheet between two aluminium skins and is not appropriate for a curtainwall on any building where the facade is required to resist fire spread.
| Core class | Typical inorganic filler | Reaction to fire, typical | Where it is normally specified | Relative cost |
|---|---|---|---|---|
| A2 non-combustible | Above 90 percent | A2-s1,d0 | High-rise facades, escape routes, hospitals, transport buildings, projects with strict insurance conditions | Highest |
| B1 flame retardant | Around 70 percent | B-s1,d0 | Low and mid-rise facades, signage, interior feature walls, projects where A2 is not mandated | Medium |
| B2 or standard polyethylene | None to low | D or E class | Not recommended for curtainwall; limited to low-risk decorative and temporary applications | Lowest |
Two practical points follow. First, the letter and the number are not the whole story. The s1 suffix refers to smoke production and the d0 suffix to flaming droplets, and a panel that reaches A2 but produces heavy smoke is a different proposition from one that reaches A2-s1,d0. Ask for the full classification, not the headline figure.
Second, the core is where manufacturing discipline is easiest to lose and hardest to see. A mineral-filled core has to be compounded to a consistent density, degassed properly, and bonded to the skins at a controlled temperature. A line running too fast, or a formulation adjusted to save filler, produces a panel that still passes a small-scale sample test taken on a good day but does not represent the shipment. This is why buyers increasingly ask not only for a classification report but for evidence of how the core is mixed and how the line controls density and bonding.
FR A2 Grade Aluminum Composite PanelA2-rated aluminum composite panel with EN 13501-1 A2-s1,d0 certification, relevant for facade specifications that require an enforceable non-combustible core class.View Product →
For specifiers working on projects where the facade must meet a non-combustible requirement, the practical route is to fix the core class in the specification text, not in a performance sentence. "Panel to achieve A2-s1,d0" is enforceable. "Panel to be non-combustible" is not, because it invites a substitution that is defensible in a meeting and indefensible in a fire test.
In a stick system, mullions and transoms are cut and assembled on site, and the infill is installed into the frame piece by piece. It is flexible and economical for low-rise and irregular geometry, but it depends heavily on site labour quality. For composite panels, the practical consequence is that panel flatness and edge tolerance have to be tight enough that site-assembled joints still line up. A tolerance that is easy to hide in a factory jig becomes visible when the frame is assembled in the open air.
Unitized curtainwalls are assembled in a factory into full-storey units and lifted into place. The quality control advantage is real, and so is the panel requirement: every unit must be dimensionally identical, because it will sit next to a unit built weeks later. Composite panels for unitized systems need consistent thickness, consistent camber and a return detail that can be jigged. This is where a stable production line matters more than a low price per square metre.
A rainscreen accepts that some water will get past the outer skin and manages it: a drained cavity, a continuous air barrier behind, and openings sized to equalise pressure. Composite panels work well here because they can be formed into cassette or tray shapes with folded returns, and because the low weight keeps the secondary framing light. The critical detail is not the panel but the cavity depth and the continuity of the barrier behind it.
Ladder systems use horizontal rails spanning between vertical mullions, with the infill supported on the rails. They suit long horizontal panel modules and are common where the design calls for strong horizontal banding. The panel span between rails becomes the governing dimension, so panel stiffness, not just fire class, enters the decision.
Across all four, one rule holds: the panel should be designed as part of the system, not as a product dropped into a generic frame. A panel that is adequate in a rainscreen cassette may be marginal in a stick system with a 1.5 m span and high suction pressure, for the simple reason that the support conditions are different.
Specification sections for curtainwalls are long, but a small number of entries do most of the work. Reading them in the right order saves a great deal of rework.
A useful habit is to convert each of these into a question for the panel supplier before the order, not after. What is the panel's flatness tolerance over a 1.5 m straightedge? What is the thickness tolerance across a 1220 mm width? What is the permissible joint width variation when the ambient temperature swings 60 degrees between installation and summer? A supplier who can answer these in numbers is a supplier who has measured them.
It is also worth separating requirements that are product properties from requirements that are system properties. Fire classification of the core is a product property. Resistance to water penetration is a system property that the panel can only support. When a facade fails a site test, the two are frequently confused, and the panel supplier is asked to solve a drainage problem that belongs to the frame design.
Understanding the line helps a buyer ask better questions, because most panel defects trace back to a specific station.
The process starts at the uncoiler, where aluminium coil is fed into a tension levelling unit. Levelling matters more than it looks: residual stress in the coil becomes visible camber in the finished panel, and no amount of downstream pressure will remove it. From there the sheet passes through pretreatment, which cleans and converts the surface so the adhesive can bond chemically rather than mechanically.
The core is prepared separately. Mineral-filled A2 compound is dry-mixed to a controlled density, then fed into an extruder that melts and meters it into a uniform sheet between the two aluminium skins. The sandwich then passes through a laminating and calendering section where heat and pressure complete the bond, followed by a cooling section that must remove heat evenly. Uneven cooling is a classic cause of internal stress and long-term bowing.
After cooling, the continuous strip is trimmed, flattened through a three-roller levelling unit, measured for thickness, covered with protective film, and cut to length. Every one of those stages has a tolerance, and the finished panel's flatness is the sum of them.
A2 Non-combustible Metal Composite Panel Production LineContinuous production line for Class A2 inorganic-core metal composite panels, suited to reviewing forming tolerance and automated process control.View Product →
For a panel manufacturer or for a buyer auditing a supplier, five checks cover most of the risk:
This is also where the equipment choice becomes a business decision for the panel producer rather than a technical curiosity. A line designed for A2 mineral cores has to handle a much higher filler load, more abrasive compound, and tighter temperature control than a standard polyethylene line. Retrofitting a standard line to run A2 material usually produces a panel that meets the letter of a specification on the sample and struggles to hold it across a production run. Producers who intend to sell into regulated markets generally start with a line specified for non-combustible core from the beginning.
Fire documentation is where the gap between a good panel and a compliant facade is widest. Three layers of evidence usually exist, and they answer different questions.
The first layer is reaction-to-fire classification of the product. In Europe this is a classification report under EN 13501-1 supported by test data, typically from EN ISO 1182 for non-combustibility and EN ISO 1716 for calorific value, plus a single burning item test for the composite. In China the equivalent route runs through GB 8624. In the United States, ASTM E84 and NFPA 285 appear in different roles. What this layer proves is how the material itself behaves when exposed to a defined heat source.
The second layer is a full-scale facade or system test. NFPA 285 in the United States and BS 8414 in the United Kingdom address the behaviour of the whole assembly, including cavities, insulation and the junction at the floor slab. A composite panel with an A2 core can perform very differently depending on what sits behind it and how the fire stop is detailed. A product certificate does not, and cannot, cover that.
The third layer is project-specific documentation: the actual product name and thickness, the manufacturing site, the date of the test relative to the formulation, and a declaration that the formulation has not changed since. This is the layer buyers skip, and it is the one that determines whether the certificate applies to what arrives on site.
Two habits reduce the risk considerably. First, ask for the classification with all suffixes, plus the test standard and the report number, and check that the report names the product family rather than a generic description. Second, ask whether the core formulation has changed since the report date, and get the answer in writing with a signature attached. A supplier who hesitates on that question has told you something useful.
Price per square metre is the least informative number in a composite panel quotation. The useful comparison is landed cost at the point of installation, which includes coating system, protective film, packing, freight damage rate, and the cost of the rejects that arrive at the bottom of the container.
Four commercial variables deserve attention before price.
Coating system. Polyester is fine for interior and low-exposure work; PVDF or FEVE is the norm for exterior curtainwall where colour retention matters over 15 to 20 years. The visible difference after a decade is not subtle.
Protective film. Film is not free and it is not neutral. It has a shelf life and a removal window, and film left on a panel in direct sun past its window becomes extremely difficult to remove. Confirm the film type and the removal deadline in the purchase order.
Capacity and lead time. A supplier quoting four weeks on an A2 order while running a standard polyethylene line is either planning to buy in, or planning to substitute. Ask about the core line, not just the cutting line. Established manufacturers usually welcome the question because it separates them from traders.
Who you are actually buying from. In this market, the party you contract with may be a manufacturer, an equipment supplier, a wholesaler, or an export trading arm of a production company. None of these is inherently better, but the obligations differ. A manufacturer controls the process and can change a formulation. A wholesaler controls stock and can change a source. Know which one is answering your technical questions, and make sure the entity named on the certificate is the entity named on the contract.
Useful questions to put in writing include: which factory will produce the panels; what is the core line's rated output and current utilisation; what is the thickness and flatness tolerance guaranteed in the contract; what is the reject policy and who pays freight on replacements; and what documentation ships with each batch.
On the delivery side, project-based facade work rarely fits a catalogue. Installation sequence, unit numbering, packing sequence by floor, and site support all affect the programme as much as the panel price does. Our project services overview explains how a line or a panel supply is typically scoped, scheduled and supported after the order, which is often the part of the quotation that is hardest to compare between suppliers.
Most composite panel problems that appear in the first two years are installation problems, not manufacturing problems. A short list covers the majority.
Cleaning is straightforward but not risk-free. Mild pH-neutral detergent, a soft brush, and plenty of water is the standard method. Abrasive pads, strong alkaline cleaners and solvent blends can dull the coating or attack the sealant. On a facade with a PVDF finish, the coating will usually outlast the sealant, so the maintenance schedule should be built around sealant inspection rather than around repainting.
Inspection intervals of 12 months are typical for the first three years, then every two to three years depending on exposure. The checks worth making are joint width against the design value, sealant adhesion by hand probe, evidence of water tracking behind the panel, and fixing condition at accessible locations.
Replacement is where the original design decision pays off. If the system was detailed with removable pressure plates or a glazed-in panel, a single damaged unit can be replaced from a scaffold in under an hour. If the panel was captured behind a fixed frame, replacement may mean dismantling several adjacent units. That difference is decided at specification stage and is almost never revisited, which is why it is worth raising while the drawings are still open. For producers planning to supply replacement panels years after the original order, keeping the coating colour and the core formulation on record is a commercial asset, not an administrative chore.
Aluminum Honeycomb Composite Panel Production LineAutomated continuous line for aluminum honeycomb composite panels, useful for producers planning controlled output and long-term replacement supply.View Product →
Mistake six deserves a note for producers rather than buyers. As more projects require A2 cores and more fabricators enter the market, the ability to demonstrate a controlled process becomes a sales asset. Manufacturers who can show the compounding, the density record and the bonding data close specification reviews faster than those who can only show a certificate. In a market where a wholesaler can source the same panel from three factories, process evidence is one of the few real differentiators.
A curtainwall is an outer building envelope that hangs from the structure and carries no floor load. It keeps weather out, lets light in, and moves with the building rather than resisting it. Because it is non-structural, its performance is judged on water tightness, air leakage, movement tolerance and fire behaviour rather than on strength in the traditional sense.
No, but it is required more often than many project teams expect. The trigger is usually building height, occupancy type, distance to the boundary, or an insurer's condition rather than a single national rule. A low-rise building with generous separation may accept a B1 flame-retardant core; a high-rise with an escape route running along the facade usually will not. The correct approach is to check the applicable code and the insurer's requirement for that specific building, then specify accordingly.
In some jurisdictions and under some conditions, yes, particularly where a full-scale facade test has been passed for the specific assembly. In many others, no. The practical risk is that B1 and A2 panels are visually indistinguishable, so a substitution made on site is hard to detect afterwards. That is one reason specifiers increasingly fix the core class by product name, and one reason buyers ask for batch-level documentation rather than a project certificate.
4 mm is the most common thickness for facade work, with 0.3 mm to 0.5 mm skins on each side. Thicker panels, typically 5 mm or 6 mm, appear where span between supports is large or where flatness requirements are severe. The decision is driven by wind load, support spacing and visual criteria, not by fire performance, which is a function of the core rather than the thickness.
A curtainwall runs continuously in front of the floor slab, so the slab edge is hidden and the facade is a single skin. A window wall sits between slab edges, so the slab is visible from outside and the system is broken at every floor. Curtainwalls generally need more movement accommodation and a continuous fire stop at each floor line; window walls are simpler but architecturally more fragmented.
Ask for the classification report with all suffixes, the test standards used, the report number, and the product family named in it. Then ask whether the core formulation has changed since the report date, and request a written declaration. Finally, ask for core density records from a recent production batch. A supplier with a genuine A2 line will have all of this available; a supplier buying on the open market usually will not.
Coating colour and system, core class, panel thickness, protective film specification, and whether the panels need routing or cassette forming. Standard colours in A2 at 4 mm from stock can move quickly; custom PVDF colours on a non-standard thickness typically need a coating run, which is where the weeks accumulate. Ordering film and coating together with the panels, rather than after, avoids the most common schedule slip.
The aluminium and the PVDF coating are usually the longest-lived elements, often performing well beyond 20 years in normal exposure. Sealants, gaskets and fixings are the shorter-lived components and should be treated as scheduled maintenance items. In coastal or heavily polluted environments, inspection intervals should be shortened and bracket isolation checked early, because galvanic corrosion at fixings is the failure mode that shortens facade life most often.
A curtainwall succeeds when the system and the panel are specified as one thing. The frame decides how movement is absorbed and how water is drained; the panel decides fire behaviour, dead load and the visual flatness that everyone notices first. Treating the panel as a commodity bought at the end of the process is how projects end up with a facade that meets a sample and not a specification.
For buyers, the practical sequence is short. Fix the fire classification with full suffixes. Fix the thickness, the coating system and the tolerances in numbers. Confirm which entity manufactures and which entity certifies. Ask for production evidence rather than only a certificate. Then compare landed cost, not price per square metre.
For producers, the same sequence reads differently but points the same way. A line built for mineral cores, with controlled compounding, even cooling and reliable levelling, is what allows a supplier to answer those questions without hesitating. In a market where panels look identical from the street, the difference is entirely in what can be documented.