Extrusion Type Zero Water Absorb A2 Noncombustible Metal (Aluminum)Composite Panel Production Line
Property Standard Value
Total thickness GB/T 17748-2008 2mm / 3mm / 4mm / 5mm / 6mm
Aluminum skin thickness GB/T 17748-2008 0.2mm / 0.3mm / 0.4mm / 0.5mm
Width — ≤2000mm (customizable)
Fire classification GB 8624-2012 A2-s1,d0
Fire classification EN 13501-1 A2-s1,d0
Fire classification BS 476-6 & 7 Class 0 + Class 1
Surface burning ASTM E84 Class 1 (FS ≤25, SD ≤50)
Facade full-scale fire NFPA 285 PASS
Peel strength GB/T 17748 ≥ 120 N/mm
Flexural strength GB/T 17748 ≥ 150 MPa
Face coating — PVDF / PE / Custom
A2 Core Granules
Property Value
Composition Inorganic content ≥90%
Flame retardancy A2 rated
Processing Twin-screw

A coil that leaves the final rinse with a bright, water-break-free surface will hold a 25 micron PVDF topcoat through twenty years of façade exposure. The same coil, painted with an identical batch of the same paint but rinsed in water sitting at 80 microsiemens per centimetre c...
View MoreA curtainwall carries no floor load. It hangs off the slab edge, seals the envelope, and hands wind, rain and thermal movement back to the frame. That single fact explains most of the arguments that appear later in a facade package, and most of the cost as well. The short answer...
View MoreFour Roller Embossing Machine: The Short Answer A four roller embossing machine with quick-change embossing rollers lets a coil processing line switch between wood grain, stone, leather and custom textures with a shorter stoppage and a lower roller-replacement burden than a fixe...
View MoreA coil of 0.6 mm aluminum goes into a multi-roll leveler and comes out of an embossing line carrying a stucco texture that hides fingerprints, softens glare and adds a little stiffness to the sheet. That small change in surface is why an Embossing Line so often sits at the front ...
View More