B1 grade fireproof core coil is a high-performance core material designed for building decoration composite materials, made by special formula and advanced technology. This product has fireproof performance, good processing adaptability and stable physical properties, and is widely used in fireproof aluminum-plastic panels, decorative composite panels and other fields. B1 core coil uses composite flame retardant, has fireproof performance, can be composited with a variety of metal substrates, can adapt to a variety of composite processes such as hot pressing and cold pressing, and achieves a combination of fireproof performance and processing performance.

Inquiry
  • FR B1 Core Coil
  • FR B1 Core Coil

1. Excellent flame retardant performance (B1 grade)
Standard certification: It complies with the B1 grade (flammable material) in the national standard GB 8624-2012 "Classification of Combustion Performance of Building Materials and Products". It can effectively inhibit the spread of flames when encountering fire and extinguish itself when away from the fire.

Flame retardant mechanism: By adding inorganic flame retardants (such as aluminum hydroxide, magnesium hydroxide) or modified polymer layers, the high temperature resistance and flame retardancy of the core material are improved.

2. Lightweight and high strength, stable structure
Multi-layer composite structure: usually composed of aluminum foil (outer layer) + flame retardant core material (polyethylene PE or special polymer) + protective layer, it has both the strength of metal and the flexibility of plastic.

Light weight: lighter than pure metal sheets, reducing building load, easy to transport and install. 3. Environmental protection and safety
Low smoke and low toxicity: less smoke production and low toxic gas release during combustion, in line with green building requirements.

Recyclable: Aluminum and some plastics can be separated and recycled to reduce environmental burden.

Our Proven
Management System

By obtaining numerous authoritative certifications both domestically and internationally, it has injected strong impetus into the development of the enterprise.

About Us

Zhangjiagang Hongyang Machinery Equipment Co., Ltd. is a national high-tech enterprise specializing in the R&D and manufacturing of intelligent equipment for metal composite materials, providing systematic solutions for the global construction materials industry. As a drafting unit of the 《Non-Combustible Metal Composite Panels for Architectural Decoration》 and a standing council member of the Metal Branch of China Building Materials Federation, the company’s core products encompass three major technological systems: Fire-resistant aluminum composite panel production lines, aluminum honeycomb core machine and aluminum honeycomb core metal composite panel production lines, and multifunctional customized metal composite panel production lines. These cover 12 categories of high-end production lines, including A2/B1-grade fire-resistant materials, 3D aluminum-core metal composite panels, and aluminum honeycomb series products.
Supported by the Suzhou Engineering Technology Research Center and Jiangsu Provincial Graduate Workstation, the company has established three technological platforms: precision transmission control, intelligent process systems, and modular design. Its equipment has been exported to 45 countries and regions, including Europe, the U.S., the Middle East, and Asia-Pacific, serving 14 of the world’s top 20 metal composite material manufacturers. Certified with ISO 9001 Quality Management System and CE Certification, the company offers a 48-hour global emergency response and reduces equipment commissioning cycles by 30% compared to industry standards. It holds 70 core patents.
Upholding the philosophy of “Quality as the Foundation, Pursuit of Excellence,” the company continuously drives technological innovation and industrial upgrading in the metal composite materials sector, striving to become a globally integrated service provider for metal composite equipment. 

News

Contact us now